STUD MATERIAL ALUMINUM STAINLESS STEEL
Grade — 5000 Series AISI grade 302 HQ
MECHANICAL PROPERTIES Tensile 45,000 psi (min) Tensile .....85,000 psi (min) Yield. 40,000 psi (min)
Yield. 25,000 psi (min)
SADDLE MATERIAL Nylon 6/6
MECHANICAL PROPERTIES Call for Details

TO ORDER OR SPECIFY, GIVE:

Product Code .................................................. CT WT

Material .................................................. Specify

WIRE TIE DOWN STUDS MECHANICAL PROPERTIES

PROPERTY ASTM METHOD TEST CONDITION UNITS NYLON 06/6
Tensile Strength D638 +73°F; 50% RH kpsi 11.2
Elongation at Break D638 +73°F; 50% RH % >=300
Yield Strength D639 +73°F; 50% RH kpsi 8.5
Shear Strength D732 Dry as Molded (DAM) kpsi 9.6
Deformation Under Load D621 2,000 psi; +122°F; DAM % 1.4
IZOD Impact D256 +73°F; 50% RH ft lb/in 2.1
Tensil Impact Strength D1822 +73°F; Long Specimen; DAM ft lb/in 240
Melting Point D789 Fisher-Johns °F 491
Thermal Linear Expansion D696 DAM in/in/°F TBD
Thermal Conductivity  - DAM Conche-Fitch BTU-in/h*ft*°F 1.7
Brittleness Temperature D746 50% RH °F -85
Oxygen Index D2863 DAM 0% 28
Oxygen Index D2864 50% RH 0% 31
UL Flammability UL 94 DAM - V-2
UL Flammability UL 95 50% RH - V-2

 

NYLON 6/6 NBS SMOKE GENERATION
  SPECIFIC OPTICAL DENSITY
SAMPLE THICKNESS UL FLAMMABILITY ENERGY SOURCE AT MAXIMUM SMOKE ACCUMULATION AT 2 MINUTES
1/16” 94 V-2

Radiant

(2.5 watts/sq. cm)

13 0
1/8” 94 V-2 Radiant Plus Flaming Gas Jets 26 1

 

NYLON 6/6 TEMPERATURE INDEX
MINIMUM THICKNESS ELECTRICAL (°C) MECHANICAL W/O IMPACT (°C) HOT WIRE IGNITION (SEC)
0.028 125 65 11.8
0.058 125 85 15

 

NYLON WIRE TIE MECHANICAL DIMENSIONS   RETAINING STUD
  INCH MM   MATERIAL: 302 HQ SS; Ultimate Tensile 85 KPSI
HEIGHT 0.39 9.9   SIZE: Equivalent to U.S. #10
LENGTH 0.875 22.22   CHEMISTRY
WIDTH 0.625 15.87   C 0.017 Mo 0.05 Ni 9.54 Co Trace
SLOT HEIGHT 0.09 2.29   S 0.001 Mn 0.83 Cu 3.07 PPM 155
SLOT WIDTH 0.325 8.26   Cr 17.5 Si 0.32 P 0.024 Fe Remainder
Unit of Measure